ASM Material Data Sheet -
Composition information provided by the Aluminum Association and is not for design. Key Words: UNS A95052; ISO AlMg2.5; Aluminium 5052-H32; AA5052-H32
We are more than an aluminium alloy solution provider.
Do you need consumer aluminium alloy products or learn more info about aluminum alloy prices?
Composition information provided by the Aluminum Association and is not for design. Key Words: UNS A95052; ISO AlMg2.5; Aluminium 5052-H32; AA5052-H32
Alloy 5052 is not hardenable by heat treatment. It can be significantly hardened by cold work (e.g. by cold rolling) and various “H” tempers are produced – most commonly H32 (1⁄4 Hard) and
Aluminium 5052 is known for its great workability allowing tight bend radii of 1.5T, it is a high strength non heat treated alloy and is corrosion resistant which makes it ideal for
5052 is the aluminum alloy most suited to forming operations, with good workability and higher strength than that of either 1100 or 3003. 5052 is not heat-treatable, but is stronger than most
Alloy AA 5052. Out of the non-heat-treatable grades, Alloy AA 5052 is one of the higher strength alloys with a fatigue strength that’s greater than most other aluminium grades. It has good
Aluminium alloy 5052 has very good corrosion resistance to seawater and marine and industrial atmosphere. It also has very good weldability and good cold formability. It is a
5052 is an aluminium–magnesium alloy, primarily alloyed with magnesium and chromium. 5052 is not a heat treatable aluminum alloy, but can be hardened through cold working. [2] Chemical properties. The alloy composition of 5052 is: [2] Magnesium - 2.2%-2.8% by
Hardness. The hardness of Aluminium Alloy 5052 varies by temper, with values such as B17 for H32, B31 for H34, and B60 for H38, indicating the material’s resistance to deformation and wear. Stress-Strain Behavior. Aluminium Alloy 5052 can absorb energy before breaking. It shows a linear elastic region, followed by plastic deformation
The Rockwell hardness scale measures the overall hardness of a metal. Metals with higher Rockwell hardness values will be harder than metals with lower Rockwell hardness values. Aluminum 5052 sheets and plates are highly formable and have more strength than 1100 and 3003 aluminum plates and sheets. They are easy to weld and resist corrosion
The properties of 5052 aluminum include 19 common variations. This page shows summary ranges across all of them. For more specific values, follow the links immediay below. Brinell Hardness. 46 to 83. Elastic (Young\'s, Tensile) Modulus. 68 GPa 9.9 x psi. Elongation at Break. 1.1 to 22 % Fatigue Strength. 66 to 140 MPa 9.5 to 20 x 10
This step increases the metal’s strength and hardness. Comparison Chart. Property 5052 Aluminum 6061 Aluminum; Heat Treatmen Non-heat treatable: Heat treatable (T6 temper common) Strengthening: 5052 aluminum is more readily available and easier to fabricate, leading to lower overall fabrication costs. On the other hand, the higher
5052-H24 aluminum is 5052 aluminum in the H24 temper. To achieve this temper, the metal is strain hardened, and then partially annealed, to a strength that is roughly halfway between annealed (O) and full-hard (H28). Brinell Hardness. 67. Elastic (Young\'s, Tensile) Modulus. 68 GPa 9.9 x psi. Elongation at Break. 8.0 % Fatigue Strength
5052 is the aluminum alloy most suited to forming operations, with good workability and higher strength than that of either 1100 or 3003. 5052 is not heat-treatable, but is stronger than most of the 5xxx series of aluminums. Hardness Rockwell | Brinell: N/A | 47: B17 | 60: B31 | 68: Elongation at Break Percentage: 22%: 12%: 10%: Modulus of
Aluminum 5052 is an aluminum alloy with magnesium as the primary alloying element, supplemented with a small chromium addition. It has good formability when in the fully soft, annealed temper and can be work-hardened to fairly high strength levels. It is commonly used in a multitude of engineering
Known for being one of the easiest types of aluminum to weld, 5052 is also recognized for its ability to resist salt water. It\'s widely used for the bodies of boats, buses, trucks, and trailers, as well as for chemical drums.. Bars are saw cut to the widths and lengths listed.. For technical drawings and 3-D models, click on a part number. Certificates with a traceable lot number are
Aluminium 5052: 5052 H32, also known for good formability, has a higher elongation of around 12.3%, Aluminium 5052: 5052 H32 has a Brinell hardness of 60, making it relatively harder and more wear-resistant. Aluminium 3003: 3003 H14 has a Brinell hardness of 40, making it softer and easier to work with than 5052. Corrosion
Known for being one of the easiest types of aluminum to weld, 5052 is also recognized for its ability to resist salt water. It\'s widely used for the bodies of boats, buses, trucks, and trailers, as well as for chemical drums.. Bars are saw cut to the widths and lengths listed.. For technical drawings and 3-D models, click on a part number. Certificates with a traceable lot number are
Hardness. 5052 aluminum is not as hard as some other alloys, but its blend of strength and flexibility makes it a popular choice for demanding applications. 5052 Aluminum Weldability. 5052 aluminum offers excellent weldability using various welding techniques, including TIG and MIG. This makes it suitable for structural components and
The results obtained from the experimental work indicated that the mechanical properties of aluminum alloy 5052 are affected significantly by the welding process
Aluminum 5052-H34. Subcategory: 5000 Series Aluminum Alloy; Aluminum Alloy; Metal; Nonferrous Metal. Close Analogs: Hardness, Knoop: 91: 91 Converted from Brinell Hardness Value: Hardness, Vickers: 78: 78 Converted from Brinell Hardness Value: Ultimate Tensile Strength: 262 MPa: 38000